Producer : |
|
pWPS-no. Producer : |
|
|
|
Examiner or examining body : |
|
|
|
WPQR-no. Producer : |
|
|
|
Date of welding : |
|
|
Creation of the sweat connection |
|
welding sequence |
|
|
|
|
material parameters |
Welding process/es : |
ISO 4063 - 111 |
Manual metal arc welding |
Product type : |
P |
Plate |
Execution of the weld : |
BW |
butt weld |
Material group / parent metal (Bm1) : |
1.1 / EN 10025-2 - S235JR |
Steels with a specified minimum yield strength ReH <= 275 N/mm2 |
Thickness of material (Bm1) : |
12.0 mm |
|
- / - |
Tube outside diameter (Bm1) : |
- / - |
|
- / - |
Material group / parent metal (Bm2) : |
1.1 / EN 10025-2 - S235JR |
Steels with a specified minimum yield strength ReH <= 275 N/mm2 |
Thickness of material (Bm2) : |
12.0 mm |
|
- / - |
Tube outside diameter (Bm2) : |
- / - |
|
- / - |
Thickness of weld metal : |
12.0 mm |
|
- / - |
welding position : |
PA |
flat position |
Gouging/Backing : |
ss nb |
one-side welding welding with no backing |
Sweat addition material (111) : |
ISO 2560-A-E 42 6 B 32 |
|
Manufacturer's name (111) : |
Castolin 6666 |
Castolin Europe GmbH |
Sweat addition material () : |
- / - |
- / - |
Manufacturer's name () : |
- / - |
|
shielding gas : |
- / - |
- / - |
shielding gas : |
- / - |
- / - |
backing gas : |
- / - |
- / - |
tungsten elektrode : |
- / - |
- / - |
|
technical parameter |
Preheat time / preheating temperature : |
- / - |
- / - |
redrying temperature : |
- / - |
- / - |
interpass temperature : |
- / - |
- / - |
cooling rate : |
- / - |
- / - |
Information impulse welding |
Basic volts / Pulse tension : |
- / - |
- / - |
background current / Pulse stream : |
- / - |
- / - |
|
Comments: Dated lists of process parameters are provided in the WPS000762 listed |
|
|
|
|
|
|